1.4435 Steel

Steel name: 1.4435
Diagram No.: 2380
Mat.No. (Wr.Nr.) designation: 1.4435
DIN designation: X2CrNiMo 18-14-3
AISI/SAE designation: 316 L
JIS designation: 316
Chemical composition in weight %: max. 0.03% C, 17.00-18.00% Cr, 2.50-3.00% Mo, 12.50-13.50% Ni
Steel group: Austenitic stainless steels
Properties: Stainless austenitic, chromium nickel molybdenum steel with low carbon content. 1.4435 is a more highly alloyed variant of 1.4404 and is commonly regarded as a medical grade of stainless steel due to its excellent resistance to all forms of corrosion and also due to the excel-lent surface finish that can be obtained.
Applications: Chemical industry, electronic equipment, crude oil and petrochemical industries, medical and pharmaceutical industry.
Reference: Not shown in this demo version.

Heat Treatment
Solution annealing: 1000 - 1100°C followed by rapid cooling in air or water.
Diagram note: No data

Tempering Diagram - mechanical Properties

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.