1.4436 Steel
Steel name: 1.4436
Diagram No.: 2381
Mat.No. (Wr.Nr.) designation: 1.4436
DIN designation: X3CrNiMo 17-13-3
SIS designation: 2343
AFNOR designation: Z7CND 18-12-03
Chemical composition in weight %: max. 0.05% C, 16.50-17.50% Cr, 2.50-3.00% Mo, 10.00-12.00% Ni
Steel group: Austenitic stainless steels
Properties: Stainless austenitic, chromium nickel molybdenum steel. 1.4436 is essentially a more highly alloyed ver-sion of 1.4401 and is specified when the corro-sion resistance of 1.4401 is no longer considered to be sufficient.
Applications: Medical and pharmaceutical industries, petrochemical industry.
Reference: Not shown in this demo version.
Heat Treatment
Solution annealing: 1020 - 1120°C followed by rapid cooling in air or water.
Diagram note: No data
Tempering Diagram - mechanical Properties
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.