1.2379 Steel
Steel name: CPPU
Diagram No.: 2399
Mat.No. (Wr.Nr.) designation: 1.2379
DIN designation: X153CrMoV12
Chemical composition in weight %: 1.55% C, 12.00% Cr, 0.80% Mo, 0.90% V
Steel group: Cold work tool steels
Properties: Ledeburitic 12% chrome steel, very high resistance against abrasive and adhesive wear due to a high volume of hard carbides in the steel matrix, good toughness, very good dimensional stability, high compressive strength, very good base material for PVD/CVD coating as well as nitriding due to its secondary hardening properties. Similar to AISI D2.
Applications: Cutting, punching, stamping tools, shear blades, thread rolling dies, cold extrusion dies, drawing and bending tools, flanging and straightening rolls, fine cutting tools, deep drawing tools, plastic moulds for abrasive polymers.
Reference: Not shown in this demo version.
Heat Treatment
Hardening:
1: 1000 - 1030°C, oil, pressure gas (N2), air or hot bath 500 - 550°C. See tempering diagram usually <300 C.
2: 1040 - 1080°C, oil, pressure gas (N2), air or hot bath 500 - 550°C. See tempering diagram usually >480 C.
Tempering: See the diagram.
Diagram note: No data
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.