1.2436 Steel

Steel name: CPW
Diagram No.: 2401
Mat.No. (Wr.Nr.) designation: 1.2436
DIN designation: X210CrW12
Chemical composition in weight %: 2.10% C, 12.00% Cr, 0.80% W
Steel group: Cold work tool steels
Properties: Ledeburitic 12% chrome steel, excellent wear resistance due to the high volume of hard carbides in the steel matrix, high surface hardness after heat treatment, medium toughness, dimensionally stable, high compressive strength, not secondary hardenable. Similar to AISI D6.
Applications: Cutting and drawing tools for high wear resistance, rolls with high dimensional stability, deep drawing tools, tools for wire, bar and tube production, cold shear blades for thin sheets.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 960 - 980°C, oil, pressure gas (N2), air or hot bath 500 - 550°C.
Tempering: See the diagram.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.