1.2767 Steel

Steel name: VNC4
Diagram No.: 2409
Mat.No. (Wr.Nr.) designation: 1.2767
DIN designation: 45NiCrMo16
Chemical composition in weight %: 0.45% C, 1.40% Cr, 0.25% Mo, 4.00% Ni
Steel group: Alloyed steels
Properties: Nickel alloyed cold work tool steel, good throughhardenability, good polishability, excellent toughness.
Applications: Shredder knives, cutting tools for thick materials, casing, plastic moulds, cutting and bending tools, shear knives for cutting scrap and billets.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 840 - 870°C, oil, pressure gas (N2), air or hot bath 180 - 220°C.
Tempering: See the diagram.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.