MLQ Xtra Steel

Steel name: MLQ Xtra
Diagram No.: 2442
Mat.No. (Wr.Nr.) designation: 1.2738 mod.
AISI/SAE designation: P20 mod.
Chemical composition in weight %: 0.26% C, 0.35% Si, 1.00% Mn, 1.45% Cr, 0.55% Mo, 0.60% Ni, +others
Steel group: Plastic mould steels
Properties: MLQ Xtra is a new, patented, pre-hardened mold steel grade specially designed for through hardenability, ease of machining and simple postproduction mold maintenance. It has high impact strength and temper resistance and very high thermal conductivity that improves heat extraction and reduces molding cycle times. The well-balanced chemistry assures homogeneous hardness and microstructure in very large cross sections with nearly no section hardness loss due to mass. MLQ Xtra is an excellent material for Polishing, Photo-Etching & Acid Texturing. The highquality mold steel undergoes premium refinement through either Vacuum Arc Remelting or Electroslag Remelting, thus eliminating nearly all segregation and inclusions.
Applications: Moulds
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 900 C
Tempering: See the diagram.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.