FTCo Steel

Steel name: FTCo
Diagram No.: 2480
Chemical composition in weight %: 0.53% C, 0.25% Si, 0.40% Mn, 4.00% Cr, 2.00% Mo, 1.10% V, 0.90% Co, 1.50% W, +Nb
Steel group: Tool steels
Properties: FTCo is a premium steel with high proportions of carbide-forming elements (Cr, Mo, V, W, Nb), which ensure particularly high tempering resistance and high wear resistance.
Applications: Dies and mandrels for forging applications with very high thermal and abrasive loads. Especially suitable for mandrels in high-speed forging machines. Tools in warm forming and brass processing.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1120 - 1140 °C. Vacuum hardening or salt bath hardening with oil/polymer quenching.
Tempering: 560 - 600 °C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.