HSF Steel
Steel name: HSF
Diagram No.: 2486
Chemical composition in weight %: 0.50% C, 0.30% Si, 0.40% Mn, 5.00% Cr, 1.90% Mo, 0.55% V, +Nb
Steel group: Hot work tool steels
Properties: HSF is a Cr-Mo-V-alloyed hot-work tool steel with increased C-content and special additives with special treatment to ensure good toughness properties.
Applications: Tools in fully automatic horizontal high speed forging machines. Stamps, dies and matrices in warm forging of steel alloys. Warm extrusion dies in steel forming. Round dies with flat engravings with high demands on hot wear resistance. Hot punches and shearing tools
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 1010 - 1040 °C. Air, warm bath of approx. 540 °C, Oil/polymer; Interrupt oil or polymer cooling at 230 - 280 °C or vacuum hardening.
Tempering: 540 - 680 °C.
Diagram note: No data
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.