W44 (1.2603) Steel

Steel name: W44 (1.2603)
Diagram No.: 2492
Mat.No. (Wr.Nr.) designation: 1.2603
DIN designation: 45CrVMoW5-8
Chemical composition in weight %: 0.45% C, 0.60% Si, 0.40% Mn, 1.60% Cr, 0.60% Mo, 0.80% V, 0.50% W
Steel group: Hot work tool steels
Properties: W44 is a medium-alloyed hot-work tool steel with high tempering resistance and good hot wear behavior.
Applications: Extrusion tools such as pressure discs and cleaning discs. Molding press die for light and heavy metal processing. Jaws, dies and punches in steel forming for the production of bolts, nuts and rivets under screw presses. Water cooling is possible.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1000 - 1050 °C. Oil/polymer, for low constant thicknesses also warm bath of approx. 540 °C. Interrupt oil or polymer cooling at 200 - 250 °C or vacuum hardening.
Tempering: 520 - 700 °C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.