PM823 Steel
Steel name: PM823
Diagram No.: 2501
Chemical composition in weight %: 0.84% C, 0.85% Si, 0.35% Mn, 7.70% C, 1.50% Mo, 2.45% V
Steel group: Cold work tool steels
Properties: Premium cold-work tool steel with a wide range of applications, combining very high abrasive wear resistance with good toughness and excellent compressive strength.
Applications: Shear blades. Punching, bending and forming tools. Thread rolling dies, thread rolling rolls. Straightening and profiling rolls for high toughness and wear resistance requirements. Tools for spring production. Calibration tools. Tools for pressing sheet metal with high yield strengths.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 1070 - 1090 °C. Oil or polymer quenching, warm bath of 540 °C.
Tempering: 530 - 600 °C.
Diagram note: No data
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.