HS1 Steel

Steel name: HS1
Diagram No.: 2502
Chemical composition in weight %: 0.50% C, 0.90% Si, 0.80% Mn, 8.00% Cr, 1.50% Mo, 1.70%
Steel group: Tool steels
Properties: This high Cr steel is characterized by increased wear resistance and high compressive strength with balanced toughness in both cold and hot work. Suitable for secondary hardening and use at elevated temperature. Nitriding and coating is possible.
Applications: Shear blades. Cutting and punching tools. Bending tools. Pressure and profile rollers. Segments for pressing tools.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1050 - 1080 °C. Oil, polymer, gas.
Tempering: 540 - 560 °C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.