RF (1.2083) Steel
Steel name: RF (1.2083)
Diagram No.: 2503
Mat.No. (Wr.Nr.) designation: 1.2083
DIN designation: X40Cr14
Chemical composition in weight %: 0.42% C, 0.40% Si, 0.30% Mn, 13.00% Cr
Steel group: Stainless steels
Properties: RF is a highly hardenable stainless and acid resistant steel. It is used for the production of smaller molds or inserts for the plastics industry in the processing of duroplasts and thermoplasts, where corrosive by-products may be produced. RF is through hardenable and low in distortion, has high wear resistance and high compressive strength. In the quenched and tempered state RF is very easy to polish.
Applications: Inserts and smaller injection molds under corrosive stress. Press molds in the processing of plastics.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 1000 - 1030 °C. Interrupt oil cooling at approx. 300 °C; in blast air for thin cross-sections; in warm bath of approx. 200 °C.
Tempering: 100 - 400 °C.
Diagram note: No data
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.