RM189 (1.2361) Steel

Steel name: RM189 (1.2361)
Diagram No.: 2606
Mat.No. (Wr.Nr.) designation: 1.2361
DIN designation: X91CrMoV18
Chemical composition in weight %: 0.90% C, <1.00% Si, <1.00% Mn, 19.00% Cr, 1.10% Mo, 0.10% V
Steel group: Corrosion resistant steels
Properties: RM189 belongs to the group of heat-treatable rust and acid-resistant steels. Because of the chemical composition and the associated high hardness, there is good resistance against abrasive wear.
Applications: Plastic molds. Rust-resistant hand and machine blades of all kinds. Perforated disks in meat grinders. Valve parts. Bearings and similar parts, which are exposed to increased wear in a corrosive environment.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1000 - 1050 °C, oil.
Tempering: 100 - 200 °C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.