Steel name: PK (1.2542)
Diagram No.: 2509
Mat.No. (Wr.Nr.) designation: 1.2542
DIN designation: 45WCrV7
Chemical composition in weight %: 0.45% C, 1.00% Si, 0.30% Mn, 1.10% Cr, 0.20% V, 2.00% W
Steel group: Cold work tool steels
Properties: PK is a tough cold-work tool steel for use under permanent hitting and impact stress.
Applications: Compressed air tools of all kinds, such as chisels, riveting heads, rivet dies, rivet blasters, etc. Hand chisels. Strainers. Deburring tools. Cold punches. Scrap chisels. Profile shear blades. Hot shear blades for medium temperature cutting material (gently preheat tools) and similar tools.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 880 - 920 °C. Interrupt oil cooling at approx. 150 °C.
Tempering: 100 - 350 °C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.