N400 (1.2767) Steel

Steel name: N400 (1.2767)
Diagram No.: 2512
Mat.No. (Wr.Nr.) designation: 1.2767
DIN designation: 45NiCrMo16
Chemical composition in weight %: 0.45% C, 0.25% Si, 0.40% Mn, 1.35% Cr, 0.25% Mo, 4.00% Ni
Steel group: Cold work tool steels
Properties: N400 is characterized by its high Ni content as a tough cold-work tool steel with high hardenability. N400 shows good polishability and texturing properties as well as good through hardenability.
Applications: Cutlery punching, shear blades for thick goods above 12 mm. Scrap and billet shear blades. Embossing and bending tools for heavy cold forming. Drawing jaws, large lathe punches and similar tools, which demand maximum toughness. Shrink rings, tempered as required to a strength of 1300-1600 MPa. Plastic molds.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 840 - 870 °C. Air, warm bath from 180 - 220 °C or oil, interrupt oil cooling at approx. 150 °C.
Tempering: 100 - 400 °C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.