LO-K 2690 Steel
Steel name: LO-K 2690
Diagram No.: 2524
Mat.No. (Wr.Nr.) designation: 1.2690
Chemical composition in weight %: 2.20% C, 5.00% Cr, 1.00% Mo, 4.80% V, 0.60% W
Steel group: Tool steels
Properties: Air hardening steel grade with minimum distortion upon heat treatment and highest safty against cracking in hardening. The steel offers extrem abrasion resistance due to its high carbon-vanadium content.
Applications: The inherent dimensional stability makes the steel suitable for gauges and precision measuring tools. The extreme abrasion resistance makes the steel suitable for brick moulds, shingle knives, ceramic moulds and other highly abrasive applications. Besides that the steel grade has its special application for tufting knives and looper in the carpet industry.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 950 – 980 °C, air /oil /gas-stream.
Tempering: 220 – 280 °C.
Diagram note: No data
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.