LO-QPM 4210 Steel

Steel name: LO-QPM 4210
Diagram No.: 2532
Other designation: ASP APZ10
Chemical composition in weight %: 1.15% C, 19.00% Cr, 2.10% Mo, 0.60% V, +N
Steel group: PM martensitic steels
Properties: Powder metallurgy produced martensitic Cr-steel, with high wear resistance and high corrosion resistance . For maximum corrosion resistance, the low hardness and tempering temperature should be selected.
Applications: This PM steel is used for plastic injection molding of abrasive and corrosive plastics, as well as in the food and medical industries. LO-QPM4210 is well suited for PVD coating with reduced corrosion resistance but the coating temperature should not exceed the tempering temperature.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1125 °C, oil/gas-stream/cryogenic treatment.
Cryogenic treatment: - 80 °C, 2h.
Tempering: 180 - 210 °C, 500 - 525 °C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.