LO-QPM T15+ Steel

Steel name: LO-QPM T15+
Diagram No.: 2535
Mat.No. (Wr.Nr.) designation: 1.3253
Chemical composition in weight %: 1.60% C, 4.80% Cr, 2.00% Mo, 5.00% V, 10.50% W, 8.00% Co
Steel group: PM high speed steels
Properties: High tungsten alloyed powder metallurgy high speed steel. Enhanced hardenability and increased wear resistance compared to standard high-speed steels. Very good hot hardness due to the high cobalt content.
Applications: Good suitability for PVD and CVD coating. LO-QPM 15+ is recommended for a wide range of tools such as broaches, punching tools, milling tools, twist drills, thread rolling dies and taps or inserts.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1000 - 1240 °C, depending on the selected hardening temperature.
Tempering: 560 °C, cooling down to room temperature.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.