LO-R 4125 Steel

Steel name: LO-R 4125
Diagram No.: 2538
Mat.No. (Wr.Nr.) designation: 1.4125
DIN designation: X105CrMo17
AISI/SAE designation: AISI 440 C
Chemical composition in weight %: 1.10% C, 17.00% Cr, 0.70% Mo
Steel group: Martensitic stainless steels
Properties: Martensitic stainless steel with best edge holding ability.
Applications: It is used for all kind of shaped and flat knives in the food processing industry, e.g. cutters for frozen goods, carcass-cleaving knives for cattle and pork, perforated discs and other accessories for mincing machines, shaped knives for the fish-processing industry. Compared to grade AISI 440 B (Mat.No. 1.4112) this steel grade offers a slightly higher hardenability, but at a reduced corrosion resistance.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1020 – 1040 °C, oil /gas-stream.
Tempering: 220 – 280 °C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.