LO-S 3247 Steel

Steel name: LO-S 3247
Diagram No.: 2542
Mat.No. (Wr.Nr.) designation: 1.3247
DIN designation: HS 2-9-1-8
AISI/SAE designation: AISI M42
Chemical composition in weight %: 1.10% C, 4.00% Cr, 9.50% Mo, 1.10% V, 1.50% W, 8.00% Co
Steel group: High speed steels
Properties: High-Speed-Steel with high carbon content on molybdenum base with good grindability due to its low V-content. The high cobalt content installs a good red hardness resp. tempering resistance.
Applications: The steel is mainly used for drills, broaches, milling cutters, circular saw blades, when under working conditions the cutting edges are forced to high temperature loads. In the field of Cold-Work-Steels the grade is used for high loaded thread rolling dies and cold extrusion rams.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1160 – 1190 °C, oil /gas-stream /salt bath (550 °C).
Tempering: 540 – 560 °C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.