Steel name: LO-W 2344 SFS
Diagram No.: 2551
Mat.No. (Wr.Nr.) designation: 1.2344
DIN designation: X40CrMoV5-1
AISI/SAE designation: H13
Chemical composition in weight %: 0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 1.00% V
Steel group: Hot work tool steels
Properties: Hot-Work-Steel with good tempering resistance, hot wear resistance, toughness and insensibility against heat-checking.However, the steel should not be forced to strong water cooling during operational use.
Applications: It is a universally applicable steel grade, used e.g. for metal-extrusion tools, tools in die casting, press forging dies, tools in plastic moulding, shear blades for hot shearing as well as for cold shearing operations. The steel grade is matching the requirements and technical specifications of the metal-extrusion industry and the die-casting industry.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1010 – 1030 °C, air /oil /gas-stream.
Tempering: 550 – 620 °C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.