BeyLos 2714 Steel
Steel name: BeyLos 2714
Diagram No.: 2563
Mat.No. (Wr.Nr.) designation: 1.2714
DIN designation: 56NiCrMoV7
AISI/SAE designation: L6
AFNOR designation: 55NCDV7
Chemical composition in weight %:
Steel group: Plastic mould steels
Properties: BeyLos 2714 is an alloy steel grade designed for the manufacture of dies, moulds, punches and other components subjected to high working temperatures and for high quality surface finishes. BeyLos 2714 is also suitable for plastic moulding applications, where high mechanical properties are required and it is recommended for processing transparent melts and for large-surface plastic parts.
Applications: BeyLos 2714 is suitable for the following applications: Large sized die blocks; plastic moulds; moulds subjected to low pressure; chill moulds for gravity casting; containers for die-casting presses;bolsters / die holders; sleeves for extrusion presses; injection moulds.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 850°C, air, vacuum cooling, salt bath, polymer, water quench.
Tempering: See the diagram.
Diagram note: No data
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.