EskyLos 2002 Steel

Steel name: EskyLos 2002
Diagram No.: 2567
DIN designation: ~28MnCrNiMo6-5-4
Chemical composition in weight %: 0.20-0.30% C, 0.20-0.50% Si, 1.40-1.70% Mn, 1.20-1.60% Cr, 0.55-0.75% Mo, 1.00-1.30% Ni
Steel group: Plastic mould steels
Properties: EskyLos 2002 is a special and innovative pre-hardened steel, suitable for the manufacture of big size injection moulds. EskyLos 2002 is obtained through a special 'super clean' manufacturing process and special heat treatments. EskyLos 2002 is normally supplied in the pre-hardened condition with a surface hardness of 360-400 HB.
Applications: Plastic moulding: Injection molds for long run productions; Injection molds for reinforced plastics; Injection molds for plastic pieces with elaborated graining (double gloss, geometric design), Injection molds for plastic pieces with elevated smoothness (transparent, painted), Lens quality polishing: prototype and short productions,Medium and big sized moulds for the automotive industry; Moulds for the food industry;, Compression molds, Bolsters.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 950 °C, polymer or water quench.
Tempering: See the diagram.
Diagram note: Tempering curve of a sample which has been austenitised at 950 °C.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.