EskyLos HiMo Steel

Steel name: EskyLos HiMo
Diagram No.: 2575
Mat.No. (Wr.Nr.) designation: ~1.2344/~1.2343
Chemical composition in weight %: 0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, <0.015% P, <0.003% S, 4.80-5.50% Cr, 2.00-2.40% Mo, 0.40-0.70% V
Steel group: Hot work tool steels
Properties: EskyLos HiMo is the new version of the high alloyed Chromium-Molybdenum-Vanadium Hot Work Tool steels family. It was developed by Lucchini RS starting from the experienced EskyLos® 2344 grade, increasing the Molybdenum (Mo) content and adding special micro-alloying elements such as Tungsten (W). It’s designed for the most demanding high pressure Light Alloys (Al-Mg) die casting dies, EskyLos®HiMo fully meets the European specifications SEP 1614.96 concerning the annealed microstructure and banding segregation and VDG M82-1993 concerning the Impact capability testing, in terms of testing and requirements.
Applications: High pressure Aluminium/Magnesium die casting moulds; Moulds for low pressure Aluminium die castings; Moulds for Aluminium gravity die castings;
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1010-1030°C, air, vacuum cooling, salt bath, polymer in H2O.
Tempering: See the diagram.
Diagram note: Tempering curve of a sample austenitised at 980 °C. The diagram shows values obtained after the second temper.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.