EskyLos 2083 Steel
Steel name: EskyLos 2083
Diagram No.: 2576
Mat.No. (Wr.Nr.) designation: 1.2083
DIN designation: X42Cr13
AISI/SAE designation: 420
AFNOR designation: Z40C14
Chemical composition in weight %: 0.35-0.45% C, <1.00% Si, <1.0% Mn, 12.50-13.50% Cr, <0.50% V
Steel group: Martensitic stainless steels
Properties: EskyLo 2083 is a martensitic stainless steel, resistant to corrosion.
Applications: EskyLos 2083 is suitable for the following applications: Moulds for corrosive plastic materials (PVC, recycled polymers, etc.), moulds for the automotive industry (head lamp components), moulds for medical instruments, moulds for food industry products, moulds for the cosmetics industry, moulds for rubber pressing, dies and gauges for PVC extrusion, mechanical parts for extrusion presses (ex. extrusion heads).
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 980 °C, oil or water quench.
Tempering: See the diagram.
Diagram note: Tempering curve of a sample which has been austenitised at 980 °C.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.