EskyLos 2083 Steel

Steel name: EskyLos 2083
Diagram No.: 2577
Mat.No. (Wr.Nr.) designation: 1.2083
DIN designation: X42Cr13
AISI/SAE designation: 420
AFNOR designation: Z40C14
Chemical composition in weight %: 0.33-0.43% C, <1.00% Si, <1.0% Mn, 12.50-13.50% Cr
Steel group: Martensitic stainless steels
Properties: EskyLos 2083 is an advanced martensitic stainless steel, Chromium based, for plastic moulds that need resistance to wear and corrosion.
Applications: EskyLos 2083 is suitable for the following applications: Moulds for corrosive plastic materials (PVC, recycled polymers, etc.); moulds for the automotive industry and optical parts (head lamp components); moulds for medical instruments; moulds for food industry products; moulds for the cosmetics industry; moulds for rubber pressing; dies and gauges for PVC extrusion; mechanical parts for extrusion presses (ex. extrusion heads).
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 980°C - 1.040°C, water, air, gas.
Tempering: See the diagram.
Diagram note: Top: Tempering curve of EskyLos 2083 samples austenitised at different temperatures between 980°C and 1.040 °C. Bottom: The suggested temperature of tempering should be outside the not recommended tempering range of 450 – 550°C (blu range), because of their possible embrittling effects.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.