BeyLos 2329 Steel

Steel name: BeyLos 2329
Diagram No.: 2596
Mat.No. (Wr.Nr.) designation: 1.2329
DIN designation: 46CrSiMoV7
Chemical composition in weight %: 0.44-0.54% C, 0.60-0.90% Si, 0.70-1.00% Mn, 1.70-2.10% Cr, 0.25-0.45% Mo, 0.50-0.80% Ni, 0.15-0.25% V
Steel group: Alloyed steels
Properties: BeyLos 2329 is a special alloyed steel designed for the manufacture of dies, moulds, punches and other components subjected to high working temperatures.
Applications: BeyLos 2329 is suitable for the following applications: Dies subjected to low pressure, containers for die-casting presses, extrusion press blocks, sleeves for extrusion presses.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 870°C, air or vacuum cooling, salt bath or polymer in H2O.
Tempering: See the diagram.
Diagram note: Tempering curve of a sample which has been austenitised at 870 °C and quenched.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.