Steel name: BeyLos 2340
Diagram No.: 2597
Chemical composition in weight %: 0.32-0.40% C, 0.10-0.30% Si, 0.30-0.50% Mn, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.30-0.50% V
Steel group: Hot work tool steels
Properties: BeyLos 2340 is a high alloyed Chromium-Molybdenum- Vanadium Hot Work Tool steel characterised by a low Silicon content and by other special micro-alloying elements.
Applications: BeyLos 2340 lends itself to the following applications: Dies for aluminium stamping; low pressure dies; moulds for gravity casting; containers for presses; matrices for aluminium extrusion; heels for extrusion presses; jackets for extrusion presses; injection moulds; special plastic moulds for the automotive industry and optical parts (head lamp components); dies and gauges for PVC extrusion.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 980 C, air, vacuum cooling, salt bath, polymer in H2O.
Tempering: See the diagram.
Diagram note: Tempering curve of a sample which has been austenitised at 980 °C. The diagram shows values obtained after the second temper.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.