EskyLos 2344 DC Steel

Steel name: EskyLos 2344 DC
Diagram No.: 2613
Mat.No. (Wr.Nr.) designation: 1.2344
DIN designation: X40CrMoV5-1
AISI/SAE designation: H13
AFNOR designation: Z40CDV5
Chemical composition in weight %: 0.35-0.40% C, 0.80-1.10% Si, 0.30-0.50% Mn, max. 0.015% P, max. 0.003% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.80-1.00% V
Steel group: Hot work tool steels
Properties: EskyLos 2344 DC is a special high alloyed Chromium- Molybdenum-Vanadium Hot Work Tool steel designed for the manufacture of dies, moulds, punches and other components subjected to high working temperatures.
Applications: EskyLos 2344 DC is suitable for the following applications: Dies for aluminium die-casting; dies subjected to low pressure; chill moulds for gravity casting; containers for die-casting presses; dies for aluminium extrusion; extrusion press blocks; sleeves for extrusion presses; injection moulds.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1010-1030 °C, air, vacuum cooling, salt bath, polymer in H2O.
Tempering: See the diagram.
Diagram note: Tempering curve of a sample which has been austenitised at 1020 °C. The diagram shows values obtained after the second temper.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.