0.54C-17.30Cr-1.10Mo Steel

Steel name: 0.54C-17.30Cr-1.10Mo
Diagram No.: 264
Chemical composition in weight %: 0.54% C, 0.45% Si, 0.40% Mn, 17.30% Cr, 1.10% Mo, 0.10% V
Steel group: Plastic mould steels
Properties: Excellent corrosion resistance, very good wear resistance, good hardenability and high hardness after quenching.
Applications: Plastic piston, plastic nozzle, plastic mould for disposable drip chamber in dialysis machines.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 980 to 1020oC/oil
Tempering: See the diagram

Tempering Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.