30MoCrV20-7 Steel

Steel name: Ovako 499Q
Diagram No.: 2679
DIN designation: 30MoCrV20-7
Chemical composition in weight %: 0.28-0.32% C, 0.15-0.25% Si, 0.30-0.50% Mn, max. 0.025% P, max. 0.0015 S, 1.60-1.80% Cr, 1.80-2.20% Mo, max. 0.20% Ni, 0.40-0.60% V
Steel group: Tool steels
Properties: IQ-Steel is an isotropic quality ultra clean steel optimized for high fatigue strength under multi axial loading.
Applications: Ovako 499Q is a tool steel suitable for carburizing or used in quenched and tempered condition. The alloying strategy gives a high tempering resistance which make the steel suitable for using in elevated temperature applications. Ovako 499Q is produced through the Ovako IQ-process (isotropic quality) to a cleanliness comparable to VAR-remelted quality. Carburizing requires certain precautions due to the high alloying content. A low carbon po-tential should be used and pre-oxidation is recommended to enhance carbon diffusion. The strong carbide formers will give an excellent microstructural stability and excellent wear properties.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 950-1050°C Hardening of as-carburized component. Forced air / Hot oil.
Tempering: 160-600°C Tempering response see graph, air
Diagram note: Ac1=752 C, Ac3=923 C.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.