40SiCrMnMo7-6-6 Steel

Steel name: Ovako 477L
Diagram No.: 2686
DIN designation: 40SiCrMnMo7-6-6
Chemical composition in weight %: 0.38-0.42% C, 1.65-1.80% Si, 1.40-1.55% Mn, <0.020% P, 0.012-0.020% S, 1.50-1.60% Cr, 0.43-0.47% Mo, <0.30% Ni
Steel group: Alloyed steels
Properties: A medium carbon steel for quench and tempering steel with high hardenability. Ovako 477L has high tensile strength in combination with high toughness, and it is often used for large axles and machine parts. By using air– or gas-quenching it is possible to reduce the amount of quenching distortion. Additionally the use of quenching medias such as oil and salt may be avoided, which improves both safety and environment. The sulphur content is in a low and narrow range for consistent machinability.
Applications: Suitable for induction or flame hardening.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 900-950°C, in air,gas or oil.
Tempering: 160-700°C.
Diagram note: Ac1=721 C, Ac3=792 C.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.