42NiSiCrMo8-7-3 Steel

Steel name: Ovako 497Q
Diagram No.: 2687
AMS designation: 6419
DIN designation: 42NiSiCrMo8-7-3
AISI/SAE designation: 300M
UNS designation: K 44220
Chemical composition in weight %: 0.39-0.44% C, 1.50-1.80% Si, 0.60-0.90% Mn, <0.015% P, 0.001% S, 0.70-0.95% Cr, 0.30-0.45% Mo, 1.65-2.00% Ni, 0.06-0.10% V
Steel group: Alloyed steels
Properties: Ovako 497Q is an ingot cast high tensile quench and tempering steel with very high strength and toughness. Ovako 497Q is an excellent choice for shafts and machine components. The high silicon content will give an improved tempering resistance. The grade is produced with the quality class IQ (isotropic quality). This ensures a very low number of elongated sulphide inclusions which will give more isotropic properties. The high oxidic cleanliness will enable the steel to meet the same high demands as for re-melted qualities. The carbon range will give a high surface hardness after surface induction hardening.
Applications: No data
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Austenitization 860-880°C 1 h, oil.
Tempering: 200-650°C, double tempering is recommended, see the tempering diagram.
Diagram note: Ms=304 C, Ac1=744, Ac3=835 C.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.