100Cr6 Steel

Steel name: Ovako 803A
Diagram No.: 2692
Mat.No. (Wr.Nr.) designation: 1.3505
DIN designation: 100Cr6
AISI/SAE designation: 52100
JIS designation: SUJ2S
Chemical composition in weight %: 0.93-0.98% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.025% P, 0.003% S, 1.35-1.60% Cr, 0.10% Mo, max. 0.25% Ni
Steel group: Structural steel, high clean steels
Properties: 100Cr6 is a through hardening bearing steels intended for rolling contact and other high fatigue applications. In the hardened condition the high hardness, high strength and high cleanliness provides the steel with the right properties to withstand high cycle, high stress fatigue. 100Cr6 is mainly used for small and medium sized bearing components. It is also regularly used for other machine components that require high tensile strength and high hardness. The hardenability approximately corresponds to a ring with max. 17 mm wall thickness.
Applications: No data
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 830-870°C, 10-60 min,
Tempering: 160-500°C, air.
Diagram note: No data.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.