UGIMA 4028/UGI 4028 Steel

Steel name: UGIMA 4028/UGI 4028
Diagram No.: 2722
Mat.No. (Wr.Nr.) designation: 1.4028
DIN designation: X30Cr13
AISI/SAE designation: 420
Chemical composition in weight %: 0.30% C, 13.00% Cr
Steel group: Martensitic stainless steels
Properties: In the treated state, a martensitic grade combining excellent mechanical properties with good corrosion resistance on suitably polished surfaces in moderately aggressive non-chlorinated environments.
Applications: Moulds for PVC products and glassware. Mechanical engineering, transport, electronic equipment, decoration and household appliances, cutlery: shafts, pistons, liners, valves, nuts and bolts, etc. Cutting tools.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: No data
Tempering: See the diagram.
Diagram note: temperatureIndicative mechanical properties after quenching in oil at 950°C and tempering for 2 hours.

Tempering Diagram - Mechanical Properties

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.