UGIMA 4057/UGI 4057 Steel

Steel name: UGIMA 4057/UGI 4057
Diagram No.: 2724
Mat.No. (Wr.Nr.) designation: 1.4057
DIN designation: X17CrNi16-2
AISI/SAE designation: 431
Chemical composition in weight %: 0.17% C, 16.00% Cr, 2.00% Ni
Steel group: Martensitic stainless steels
Properties: Is required when chromium martensitic steels prove insufficient in terms of toughness or corrosion resistance. Good heat conduction. Low expansion. Suitable for polishing. Keeps a good hot surface condition. Mechanical strength up to 600°C. For descaling, please consult us. UGIMA grade developed according to Ugitech process in order to significantly improve its machinability (15% to 25% increase in productivity), up to diameter 115 mm.
Applications: Mechanical engineering, chemicals industry, oil and petrochemicals industry, transport, aerospace, defence, offshore. Moulds for glass bottles with appropriate heat treatment. For extrusion blow-moulded bottles in PVC with appropriate heat treatment.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: No data
Tempering: See the diagram.
Diagram note: Indicative mechanical properties after quenching in oil at 950°C and tempering for 2 hours.

Tempering Diagram - Mechanical Properties

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.