Ergste 1.4310FD/FI Steel

Steel name: Ergste 1.4310FD/FI
Diagram No.: 2728
Mat.No. (Wr.Nr.) designation: 1.4310
DIN designation: X10CrNi18-8
Chemical composition in weight %:
1.4310FD steel: 0.07-0.15% C, <1.00% Si, <1.60% Mn, <0.04% P, <0.015% S, 16.50-18.00% Cr, <0.80% Mo, 7.00-8.00% Ni
1.4310FI steel: 0.07-0.13% C, <1.80% Si, <1.70% Mn, <0.04% P, <0.015% S, 16.50-18.00% Cr, <0.80% Mo, 6.80-7.80% Ni
Steel group: Stainless steels
Properties: Ergste 1.4310FD is a stainless, austenitic chrome-nickelsteel with excellent spring characteristics. The Ergste 1.4310FD is characterized by its great work hardening whereas a high tensile strength along with very good ductile properties is achieved. The material Ergste 1.4310FI is the development of the 1.4310FD and allows even smaller bending radii. Furthermore, this material has stronger starting behavior, see also tempering diagram.
Applications: Electrical and clamping spring industry.
Reference: Not shown in this demo version.

Heat Treatment
Solution Annealing: 1000 – 1100 °C, water, air.
Tempering: max. 420 °C, air.
Diagram note: No data.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.