Ergste 9.9200GA Steel

Steel name: Ergste 9.9200GA
Diagram No.: 2729
Chemical composition in weight %: <0.030% C, 0.20% Si, 12.00% Cr, 2.00% Mo, 8.90% Ni, 1.60% Ti, <0.030% N
Steel group: Stainless steels
Properties: Ergste 9.9200GA is a precipitation hardenable 12% chromium nickel steel with outstanding corrosion resistance and impact toughness. Despite high strength this quality can be formed relatively well. By appropriate cold forming / heat treatment is a hardness of max. 51 HRC* to reach.
Applications: Surgical instruments (e.g. drills). Cutting instruments (e.g. rasps).
Reference: Not shown in this demo version.

Heat Treatment
Solution Annealing: 1,796 ± 60 °F, furnace, air.
Precipitation Hardening: 896 – 1,004 °F, holding time: ca. 4h (depending on material mass), cooling: air.
Diagram note: No data.

Precipitation Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.