Orvar 2 Microdized Steel

Steel name: Orvar 2 Microdized
Diagram No.: 2739
Mat.No. (Wr.Nr.) designation: 1.2344
EN designation: X40CrMoV5-1
AISI/SAE designation: H13
Chemical composition in weight %: 0.39% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.30% Mo, 0.90% V
Steel group: Hot work tool steels
Properties: Uddeholm Orvar 2 Microdized is a chromiummolybdenum- vanadium-alloyed steel.
Applications: For applications requiring extreme levels of toughness and ductility e.g. die casting dies, forging dies, the premium grade H13-steel, Uddeholm Orvar Supreme, is recommended.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Pre-heating temperature: 600–850°C (1110– 1560°F), normally in two pre-heating steps. Austenitizing temperature: 1020–1050°C (1870– 1920°F), normally 1020–1030°C (1870– 1885°F). Quenching media: High speed gas/circulating atmosphere. Vacuum (high speed gas with sufficient positive pressure). An interrupted quench is recommended where distortion control and quench cracking are a concern. Martempering bath or fluidized bed at 450– 550°C (840–1020°F), then cool in air. Martempering bath or fluidized bed at 180–220°C (360–430°F) then cool in air. Warm oil.
Tempering: See the diagram.
Diagram note: No data.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.