Holdax Steel

Steel name: Holdax
Diagram No.: 2759
Mat.No. (Wr.Nr.) designation: 1.2312
AISI/SAE designation: 4130–35 improved
Chemical composition in weight %: 0.40% C, 0.40% Si, 1.50% Mn, 0.07% S, 1.90% Cr, 0.20% Mo
Steel group: Alloyed steels
Properties: Uddeholm Holdax is a vacuum-degassed chromium-molybdenum-alloyed steel which is supplied in the hardened and tempered condition.
Applications: Holders/bolsters for plastic moulds and die casting dies. Plastics and rubber moulds with low requirements on polishability. Support plates. Constructional parts.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Note: The steel should be fully soft annealed before hardening. Preheating temperature: 500–600°C (930–1110°F). Austenitizing temperature: 850°C (1560°F).
Quenching media: Forced air/atmosphere (only for small tools). Oil. Martempering bath 450–550°C (840– 1020°F) max. 4 minutes, then cool in forced air.
Tempering: Choose the tempering temperature according to the hardness required by reference to the tempering graph. Temper twice with inter-mediate cooling to room temperature. Lowest tempering temperature 180°C (360°F). Holding time at temperature minimum 2 hours.
Diagram note: The diagram below is valid for small samples (15 x 15 x 40 mm) quenched in air. Austeni-tizing temperature 850°C (1560°F), 30 min. Holding time 2 + 2 h.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.