Nimax ESR Steel

Steel name: Nimax ESR
Diagram No.: 2761
Chemical composition in weight %: 0.10% C, 0.30% Si, 2.50% Mn, 3.00% Cr, 0.30% Mo, 1.00% Ni
Steel group: Plastic mould steels
Properties: Uddeholm Nimax ESR is a low carbon plastic mould steel delivered at a hardness of ~40 HRC. Uddeholm Nimax ESR is an ESR remelted version of Uddeholm Nimax, keeping the features of Uddeholm Nimax, but with improved cleanliness and homogeneity as a result of the ESR process.
Applications: The material is specifically developed for big and middle sized injection moulds with high demands on surface finish. Main applications are transparent, high gloss polished or textured moulds for use mainly within automotive, white goods, packaging and electronic industry.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Uddeholm Nimax ESR is intended to be used in the delivery condition. The hardness cannot be increased by heat treatment, but can be decreased by tempering. However, tempering is not recommended because it significantly decreases toughness even though that the hardness is reduced.
Tempering: See the diagram.
Diagram note: No data.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.