40CrMnMo7 Steel

Steel name: 40CrMnMo7
Diagram No.: 2772
Mat.No. (Wr.Nr.) designation: 1.2311
AISI/SAE designation: P20
Chemical composition in weight %: 0.38% C, 0.30% Si, 1.50% Mn, 1.90% Cr, 0.20% Mo
Steel group: Plastic mould steels
Properties: Low-sulfur mold steel supplied as heat-treated for service strength. Preferable if die sinking is to be done by spark erosion or photochemical machining or if excellent polishability is required. The usual service strength of MFR is approx. 1000 N/mm². If, in exceptional cases, a higher strength should be required, please refer to the following heat-treatment instructions.
Applications: No data
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 840–860 °C (1540–1580 °F). Oil or hot bath of 200–230 °C (390–450 °F) (for thin wall thickness).
Tempering: To service hardness as shown in the tempering diagram (min. 1 hr/25 mm thickness).
Diagram note: No data.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.