1.10C-1.0Si-0.35Mn-7.90Cr-1.50Mo-2.20V-1.20W Steel
Steel name: 1.10C-1.0Si-0.35Mn-7.90Cr-1.50Mo-2.20V-1.20W
Diagram No.: 2784
Chemical composition in weight %: 1.10% C, 1.00% Si, 0.35% Mn, 7.90% Cr, 1.50% Mo, 2.20% V, 1.20% W
Steel group: Cold work tool steels
Properties: This cold-work tool steel produced is a medium-chromium, air-hardening tool steel providing a very good combination of wear resistance and toughness.
Applications: It is available primarily in round bars for cold-work tooling applications.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 1040 to 1080 °C / air, oil or inert gas. To increase hardness by 1 to 2 HRC and dimensional stability after quenching, sub-zero treatment may be used.
Tempering: Temper immediately after quenching (when material reaches temp. 90-70 °C). At least two tempering treatments are recommended to achieve a uniform tempered microstructure. Slowly heat to reach tempering temperature. Holding time in the furnace: 1 hour for every 25 mm of workpiece thickness, but 2 hours minimum. This is followed by air cooling. Typical tempering temperatures are 150 to 550 °C.
Diagram note: Legend: Trdota-hardness, Temperatura-temperature,
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.