M50 Steel

Steel name: M50
Diagram No.: 346
UNS designation: K88165
AISI/SAE designation: M50
Chemical composition in weight %: 0.80% C, 0.30% Si, 0.70% Mn, 0.015% P, 0.015% S, 4.00% Cr, 4.50% Mo, 0.10% Ni, 1.00% V
Steel group: High speed steels
Properties: No data
Applications: M50 high speed steel has been used in a wide variety of applications in the bearing and missile industry for components which require high wear resistance and strength at elevated temperatures. It has been used for bearings in aircraft and gas turbine engines operating at service temperatures up to about 700°F (371°C).
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1100oC/No data
Tempering: See the diagram

Diagram Tempering Temperature - Mechanical Properties

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.