1.90C-20.00Cr-1.00Mo-4.00V Steel

Steel name: 1.90C-20.00Cr-1.00Mo-4.00V
Diagram No.: 347
Chemical composition in weight %: 1.90% C, 0.30% Si, 0.30% Mn, 20.00% Cr, 1.00% Mo, 4.00% V, 0.60% W
Steel group: PM stainless tool steel
Properties: No data
Applications: Steel excels in applications, which require a combination of high wear resistance and high corrosion resistance. The unique combination of properties makes this steel an excellent steel for plastic injection feed screws, barrel liners, screw tips, and mold cavities, especially for plastic resins which contain abrasive fillers. Other applications include food processing equipment, pelletizer knives, granulator knives, and high-performance custom knives.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1071-1177oC/oil, gas, vacuum, salt bath
Tempering: See the diagram
Diagram note: For vacuum furnace hardening, vacuum hardened and 4bar nitrogen gas quenched.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.