X153CrMoV12 Steel

Steel name: X153CrMoV12
Diagram No.: 362
DIN designation: X153CrMoV12
Mat.No. (Wr.Nr.) designation: 1.2379
AISI/SAE designation: D2
Chemical composition in weight %: 1.55% C, 0.30% Si, 0.35% Mn, 12.00% Cr, 0.75% Mo, 0.90% V
Steel group: 12 % ledeburitic chromium steel tool steel
Properties: No data
Applications: Threading rolls and dies, cold extrusion tools, trimming, cutting and stamping tools for sheet thicknesses up to 6 mm, precision cutting tools for sheet thicknesses up to 12 mm, cold pilger mandrels, circular-shear blades, deep-drawing tools, pressure pads and highly wear-resistant plastic moulds.
Reference: Website Deutsche Edelstahlwerke GmbH, Germany, 2010.

Heat Treatment
Hardening: 1000 – 1050oC/air, oil, salt bath
Tempering: See the diagram

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.