1.2365 Steel

Steel name: 1.2365
Diagram No.: 380
DIN designation: X32CrMoV33
Mat.No. (Wr.Nr.) designation: 1.2365
AISI/SAE designation: H10
Chemical composition in weight %: 0.30% C, 0.30% Si, 0.30% Mn, 3.00% Cr, 2.80% Mo, 0.60% V
Steel group: Tool steels
Properties: No data
Applications: This steel is suitable for dies for die-casting of heavy alloys, drawing dies, mandrels and other items for extrusion presses, internal collets, punches, tools for the production of nuts and bolts, for small hot dies, single-block dies for presses, hot shears subjected to strong thermal stresses and mandrels for hot drawing.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 990-1010oC/air, oil
Tempering: See the diagram
Diagram note: Hardening 1030oC/air.

Tempering Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.