35NiCrMo16 Steel
Steel name: 35NiCrMo16
Diagram No.: 390
DIN designation: 35NiCrMo16
Mat.No. (Wr.Nr.) designation: ~1.2766
AFNOR designation: 40NCD16
Chemical composition in weight %: 0.43% C, 0.30% Si, 0.70% Mn, 3.70% Ni, 1.70% Cr, 0.40% Mo, 0.10% V
Steel group: Tool steels
Properties: No data
Applications: This steel is particularly suitable for the manufacture of dies for hammers and rams, forming dies and punches, cutters for shearing billets, scrap and thick plates, moulds for plastics and for the manufacturing of mechanical components. It is used also for bending tools, for punching and pressing (cutlery and goldsmithing) and for hot and cold coining.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 850-880oC/air
Tempering: See the diagram
Diagram note: Hardening 870oC/air.
Tempering Diagram
Click the image to enlarge the diagram.
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.