X165CrMoV12 Steel
Steel name: X165CrMoV12
Diagram No.: 593
DIN designation: X165CrMoV12
Mat.No. (Wr.Nr.) designation: 1.2601
Chemical composition in weight %: 1.65% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
Steel group: Cold work tool steels
Applications: High performance blanking and punching dies for sheet thickness up to 5 mm; circular and straight shear blades for sheet thickness up to 4 mm; precision stamping tools; cold drawing tools; hobbing dies; flanging rolls; guide rolls; forming and sizing rollers for continuous production of steel tubes and profiles; tools for the cold forming of bolts, nuts and rivets; woodworking and similar tools.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 960 - 1010oC/oil, hot bath, air
Tempering: See the diagram
Diagram note: Sample diameter: 25 mm, hardening: 1070oC/oil.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.