X210CrW12 Steel

Steel name: X210CrW12
Diagram No.: 599
DIN designation: X210CrW12
Mat.No. (Wr.Nr.) designation: 1.2436
Chemical composition in weight %: 2.10% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 0.70% W
Steel group: Cold work tool steels
Applications: High performance blanking and punching dies (also for silicon steel sheet), circular and straight shear blades, for sheet thickness up to 2 mm; cold extrusion tools (upper and bottom dies); deep-drawing tools; tools for cold forming of nuts and rivets; hobbing dies; flanging tools; guide rolls; forming and sizing rollers for continuous production of steel profiles and tubes; forming tools for ceramics and for powder metallurgy; cutting tools for paper and plastics; broaches and similar tools.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 950 - 980oC/oil, hot bath, air
Tempering: See the diagram
Diagram note: Sample diameter: 25 mm, hardening: 970oC/oil.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.